MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
CoorsTek STATSAFEā„¢ ADC-92 Nom. 92% Alumina, Al2O3
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: CoorsTek provides state-of-the-art materials manufactured using the most cost-effective processes. CoorsTek maintains efficient, large-scale manufacturing facilities to support quick-turn prototype development and high-volume production.

Wide Variety of Manufacturing Options

  • Injection molding
  • Roll compacting
  • Extruding
  • Co-firing
  • Isostatic pressing
  • Dry pressing
  • Hot pressing
  • Tape casting
  • Slip casting
Advanced Finishing Services
  • Engineering design & support
  • Precision grinding & lapping
  • Laser machining
  • Metallizing
  • Ceramic-to-metal brazing
  • Specialized coatings
  • Threaded components
  • Precision motion components
  • Complex cleanroom assemblies

Information provided by CoorsTek.

Key Words: Al2O3 Aluminum Oxide
Vendors:
Available Properties
  • Density, ASTM-C20
  • Particle Size, ASTM-E112
  • Hardness, Vickers, ASTM-C1327, [Gpa]
  • Modulus of Elasticity, ASTM-C848
  • Flexural Strength, ASTM-C1161, 4-PT (MOR)
  • Poissons Ratio, ASTM-C848
  • Fracture Toughness, NOTCHED BEAM
  • Volume Resistivity, ASTM-D1829
  • CTE, linear, ASTM-C372
  • Specific Heat Capacity, ASTM-E1269
  • Thermal Conductivity, ASTM-C408
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.