MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
SABIC NORYL™ Resin LTA6020 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ LTA6020 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm, 5VB at 2mm, and V0 at 1.5mm. NORYL LTA6020 exhibits good dimensional stability over a wide temperature range, high heat performance, low moisture uptake, and offers long-term aging / retention of mechanical properties. It is an excellent candidate for solar / photovoltaic (PV) junction boxes and outdoor electrical enclosures.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Density, ISO 1183
  • Moisture Absorption, Injection Molding
  • Viscosity, ISO 1133, MVR cc/10 min
  • Viscosity, ISO 1133, MVR cc/10 min
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ISO 527, 50 mm/min
  • Tensile Strength, Yield, ISO 527, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Elongation at Yield, ISO 527, 50 mm/min
  • Elongation at Yield, ASTM D638, 50 mm/min
  • Tensile Modulus, ISO 527, 1 mm/min
  • Flexural Strength, ASTM D790, yld, 2.6 mm/min, 100 mm span
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Modulus, ASTM D790, 2.6 mm/min, 100 mm span
  • Flexural Modulus, ISO 178, 2 mm/min
  • Izod Impact Notched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Charpy Impact Unnotched, ISO 179/2C
  • Comparative Tracking Index, UL 746A
  • Hot Wire Ignition, HWI, UL 746A
  • High Amp Arc Ignition, HAI, UL 746A
  • High Voltage Arc-Tracking Rate, HVTR, UL 746A
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Hot Ball Pressure Test, IEC 60695-10-2, PASS
  • Hot Ball Pressure Test, IEC 60695-10-2
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Bf, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Vicat Softening Point, ISO 306, Rate B/120
  • Vicat Softening Point, ISO 306, Rate A/120
  • UL RTI, Electrical, UL 746B
  • UL RTI, Mechanical with Impact, UL 746B
  • UL RTI, Mechanical without Impact, UL 746B
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Zone 2
  • Zone 3
  • Melt Temperature, Injection Molding
  • Mold Temperature
  • Drying Temperature, Injection Molding
  • Dry Time, Injection Molding
  • Precipitation Temperature, Hopper Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.