MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Sandvik Sanicro 56 Welding wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Sanicro 56 is a low carbon nickel-chrome-molybdenum alloy of type alloy C276. It is a versatile alloy with excellent wet corrosion resistance in oxidizing and especially in reducing media. However, in oxidizing chloride containing environments alloy UNS N06022 (2.4602) is preferred while Sanicro 54 is a better matching welding consumable. Applications for Sanicro 56 are found in aggressively corrosive media such as chemical processing plants, pollution control, pulp and paper production, waste treatment and for the recovery of sour natural gas. Sanicro 56 is used for joining alloy UNS N10276 (2.4819) and other nickel-chrome-molybdenum alloys. It can also be used for dissimilar metal joining of nickel alloys, stainless steels and low-alloy steels. Sanicro 56 can be used for surfacing low alloyed steels.

Information provided by Sandvik

Vendors:
Available Properties
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Charpy Impact
  • Charpy Impact
  • Carbon, C, All-weld metal
  • Carbon, C, Filler metal
  • Chromium, Cr, Filler metal
  • Chromium, Cr, All-weld metal
  • Cobalt, Co, Filler metal
  • Iron, Fe, Filler metal
  • Manganese, Mn, All-weld metal
  • Manganese, Mn, Filler metal
  • Molybdenum, Mo, All-weld metal
  • Molybdenum, Mo, Filler metal
  • Nickel, Ni, Filler metal
  • Nickel, Ni, All-weld metal
  • Phosphorus, P, Filler metal
  • Silicon, Si, All-weld metal
  • Silicon, Si, Filler metal
  • Sulfur, S, Filler metal
  • Tungsten, W, Filler metal
  • Tungsten, W, All-weld metal
  • Vanadium, V, Filler metal
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.