| Product Description: QM 263 is a two-component, room temperature, addition cure, silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for the molding of furniture, picture frames and architectural materials. Key Features: - High durometer
- Casting resin resistance
- Fast demold time
- Excellent dimensional stability
Main Applications:- Molds for architectural application
- Molds for polyester, epoxy resin casting, and rigid or foam polyurethane
- Molds for technical articles and prototypes
- Molds for furniture and picture frame replication
Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017 |