MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
3M Dyneon™ PFE 02CZ Perfluoroelastomer Curative Masterbatch  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Product Description: 3M™ Dyneon™ PFE 02CZ is a cure accelerator masterbatch used to adjust cure speeds in HT PFE products. The base polymer is classified as FFKM per ASTM D1418.

Information provided by 3M™

Vendors:
Available Properties
  • Hardness, Shore A, 0 PFE 02CZ
  • Hardness, Shore A, 2.5 PFE 02CZ
  • Hardness, Shore A, 5 PFE 02CZ
  • Hardness, Shore A, 1.25 PFE 02CZ
  • Hardness, Shore A, 0 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Hardness, Shore A, 1.25 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Hardness, Shore A, 2.5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Hardness, Shore A, 5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Hardness, Shore A, 2.5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Hardness, Shore A, 0 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Hardness, Shore A, 5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Hardness, Shore A, 1.25 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Tensile Strength at Break, ASTM D573, 0 PFE 02CZ
  • Tensile Strength at Break, ASTM D573, 1.25 PFE 02CZ
  • Tensile Strength at Break, ASTM D573, 2.5 PFE 02CZ
  • Tensile Strength at Break, ASTM D573, 5 PFE 02CZ
  • Tensile Strength at Break, ASTM D573, 0 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Tensile Strength at Break, ASTM D573, 1.25 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Tensile Strength at Break, ASTM D573, 2.5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Tensile Strength at Break, ASTM D573, 5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Tensile Strength, 0 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Tensile Strength, 2.5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Tensile Strength, 1.25 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Tensile Strength, 5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Elongation at Break, 1.25 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Elongation at Break, 0 PFE 02CZ
  • Elongation at Break, 0 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Elongation at Break, 5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Elongation at Break, 2.5 PFE 02CZ
  • Elongation at Break, 1.25 PFE 02CZ
  • Elongation at Break, 5 PFE 02CZ
  • Elongation at Break, 2.5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Elongation at Break, 0 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Elongation at Break, 2.5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Elongation at Break, 1.25 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • Elongation at Break, 5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
  • 100% Modulus, 2.5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • 100% Modulus, 0 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • 100% Modulus, 5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • 100% Modulus, 1.25 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
  • Compression Set, ASTM D395 Method B, 1.25 PFE 02CZ, -214 O-rings, 25% Deformation
  • Compression Set, ASTM D395 Method B, 5 PFE 02CZ, -214 O-rings, 25% Deformation
  • Compression Set, ASTM D395 Method B, 2.5 PFE 02CZ, -214 O-rings, 25% Deformation
  • Compression Set, ASTM D395 Method B, 0 PFE 02CZ, -214 O-rings, 25% Deformation
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.