MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Park Aerospace Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines and spaces and larger panel sizes.

Key Features and Benefits:

  • High thermal performance
  • Self adhesive bond to foam cores
  • Superior electrical properties
  • Typical Cyanate Ester processing
  • S-glass and Quartz options

Applications:

  • Fine-Line Multilayers
  • Backplanes
  • Surface-Mount Multilayers
  • BGA Multilayers
  • MCM-L's
  • Direct Chip Attach
  • Automotive
  • Underhood Automotive
  • Wireless Communcations
  • High Speed Computing
  • Radomes and Secondary Aerospace Structure

Information provided by Park Electrochemical Corp.

Vendors:
Available Properties
  • Density, 50% resin content
  • Modulus of Elasticity, ASTM D3039, Y
  • Modulus of Elasticity, ASTM D3039, X
  • Poissons Ratio, ASTM D3039, X
  • Poissons Ratio, ASTM D3039, Y
  • Peel Strength, IPC-TM-650.2.4.8, 1 oz. Cu, after solder float
  • Peel Strength, IPC-TM-650.2.4.8, 1 oz. Cu, after exposure to process solutions
  • Volume Resistivity, IPC-TM-650.2.5.17.1, C - 96/35/90
  • Volume Resistivity, IPC-TM-650.2.5.17.1, E - 24/125
  • Surface Resistance, IPC-TM-650.2.5.17.1, C - 96/35/90
  • Surface Resistance, IPC-TM-650.2.5.17.1, E - 24/125
  • Dielectric Constant, IPC-TM-650.2.5.5.5, 50% Resin Content; Stripline
  • Dielectric Constant, IPC-TM-650.2.5.5.9, 50% Resin Content; RF Impedance
  • Dielectric Strength, IPC-TM-650.2.5.6.2
  • Dielectric Breakdown, IPC-TM-650.2.5.6
  • Dissipation Factor, IPC-TM-650.2.5.5.5, 50% Resin Content; Stripline
  • Arc Resistance, IPC-TM-650.2.5.1
  • CTE, linear, IPC-TM-650.2.4.41, Z-Axis, Alpha 1
  • CTE, linear, IPC-TM-650.2.4.41, Z-Axis, Alpha 2
  • Specific Heat Capacity, ASTM E1461
  • Thermal Conductivity, ASTM E1461, Z
  • Thermal Conductivity, ASTM E1461, X-Y
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.24c, TMA
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.25c, DSC
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.24.3, DMA (Tan d Peak)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Park Aerospace, former Park Electrochemical Corp.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.