MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Suqian Unitechem Hindered Amine Light Stabilizer 770
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: Bis(2,2,6,6-tetramethyl-4-piperidyl)sebaceate

CAS NO.: 52829-07-9

Molecular Formula: C28H52O4N2

Applications: LS770 is recommended to be used in polypropylene, impact modified PP(TPO), EPDM, polystyrene, impact polystyrene, ABS, SAN, ASA and polyurethanes and is also effective in polyamides and polyacetals.

Features/Benefits: LS770 is a low molecular weight hindered amine light stabilizer that provides excellent light stability for thick sections and films in the recommended substrates. Benefits of using LS770 include the high light-stabilizing performance, particularly in PP thick sections. It has broad compatibility and can be easily dispersed. Compared to conventional UV-absorbers, the effectiveness of LS770 is less dependent on the polymer's thickness. For this reason, the use of LS770 also provides good light stability in articles with higher specific surface, e.g. films and tapes.

Information Provided by Suqian Unitechem Co., Ltd.

Vendors:
Available Properties
  • Volatiles
  • pH, 1% suspension in water 20-25°C
  • Molecular Weight
  • Ash
  • Melting Point
  • Transmission, Visible, 425nm
  • Transmission, Visible, 500nm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.