MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Proto3000 Formlabs Silicone 40A Resin
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset; Silicone

Material Notes: Formlabs Silicone 40A Resin brings you the future of 3D printing with its groundbreaking Pure Silicone Technology™ by Formlabs. You can effortlessly create pure silicone parts in your own workspace within hours. Craft soft, flexible, and robust components using this 40A Shore durometer material with an impressive 230% elongation at break and a tear strength of 12 kN/m, ensuring your creations can endure stretching, flexing, and compression without fail. Unleash your creativity with 3D printing, combining the exceptional performance of silicone with design freedom. Craft silicone parts with remarkable chemical and thermal resistance (-25°C to 125°C), intricate details down to 0.3 mm, and complex shapes that were once impossible with traditional methods.

Characteristics/Benefits

  • Outstanding Elastomeric Performance
  • Create customized silicone parts with isotropic properties, fine features as small as 0.3 mm
  • Cost-Effective Rapid Prototyping and Low Volume Manufacturing
  • Fast and Easy Fabrication

Information provided by Proto3000

Vendors:
Available Properties
  • Tensile Strength, Ultimate
  • Elongation at Break
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.