MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Superior Die Set FORTAL® HR Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and doesn't require a very high ratio of resistance/mass. FORTAL offers machinability, high resistance to corrosion, and leads to increased productivity. FORTAL's modulus of elasticity is one third that of steel, and can absorb three times as much shock and vibration in its elastic phase. FORTAL is solution heat-treated, stabilized, artificially aged and stress relieved by stretching.

Application: FORTAL is an ideal material for all types of products and tooling since it is stronger than 1020 steels.

Information provided by Superior Die Set.

Vendors:
Available Properties
  • Density
  • Thickness, intermediate sizes also available
  • Hardness, Brinell
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Fatigue Strength, test bar (22mm diam.) notched (Kt = 3)
  • Fatigue Strength, test bar (22mm diam.) unnotched (Kt =1)
  • Shear Strength
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air, Recommended
  • Aluminum, Al
  • Chromium, Cr
  • Copper, Cu
  • Magnesium, Mg
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.