MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Lubrizol Pearlstick™ 5712 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Pearlstick™ 5712 TPU is a Polyester-Type Thermoplastic Polyurethane (TPU).

Features: It has the highest peel and green strengths and shortest open-tack time of any Pearlstick TPU resin used in adhesives. Supplied as pale amber granules, it is lightly dusted with talc. Higher heat resistance, tensile and bond strengths can be achieved with the addition of diisocyanates, peroxides, epoxies and polyfunctional amides.

Uses: Solution and melt coating.

Information provided by The 159 Corporation

Vendors:
Available Properties
  • Specific Gravity, ASTM D-792
  • Viscosity, ASTM D-1084-88, Melt
  • Brookfield Viscosity, 15% Total Solids in DMF, RVTD, Spindle n°2, 20 rpm
  • Hardness, Shore D, ASTM D-2240
  • Tensile Strength, ASTM D-412/D-638
  • Elongation at Break, ASTM D-412/D-638
  • 100% Modulus, ASTM D-412/D-638
  • 300% Modulus, ASTM D-412/D-638
  • Peel Strength, ASTM D-1876-72, T-Peel, Aluminum Foil
  • Peel Strength, ASTM D-1876-72, T-Peel, Mylar Film
  • Peel Strength, Green Strength
  • Peel Strength, Final
  • Glass Transition Temp, Tg
  • Ring & Ball Softening Point, ASTM E-28-92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lubrizol (former Noveon)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.