Temper: As Centrifugal Cast Precipitation Hardened Casting Characteristics: High – Shrinkage in Solidification; Medium - Fluidity, Drossing; Low - Gassing Fabrication Properties: Excellent Suitability – Soldering, Brazing Typical uses: Electrical Parts; Gears for Mining Equipment; Propeller Wheels; Valve Stems; Outboard Marine Components Applicable Specifications: As Sand Cast – Castings ASTM B763/B763M; Ingot - ASTM B30 |