MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Wacker Vinnapas® 401 Vinyl Acetate-Ethylene Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® 401 is a poly(vinyl alcohol) stabilized vinyl acetate-ethylene copolymer dispersion with a glass transition temperature (Tg) of -15 °C. It was developed to offer easy clean-up, long open time and excellent film flexibility.

Properties: VINNAPAS® 401 is used as a base for adhesives and has an excellent balance of very good wet tack, speed of set, adhesion, and heat resistance. It has a high thickening response to plasticizer and a long open time. The low Tg of the dried film provides excellent cold temperature flexibility. Compared to VINNAPAS® 400, this dispersion offers cleaner machining, easier clean up and is suitable for a variety of roll, extruder, and spray applications. VINNAPAS® 401 is especially suited for non-contact extrusion machine configurations.

Application: VINNAPAS® 401 can be used to bond a variety of substrates including but not limited to coated and uncoated paper, cellulose acetate, polystyrene, poly(vinyl chloride) (PVC), and poly(vinylidene chloride). It is recommended for use in high-speed packaging and envelope applications where rapid setting speeds, good machining, and easy-clean up properties are required. The long open time helps to prevent premature drying under conditions of prolonged exposure to air especially on large diameter applicator rolls and non contact extrusion nozzles. The higher level of ethylene in the polymer acts as an internal plasticizer which provides flexibility and reduces or eliminates the need for plasticizer in many applications. Due to the low Tg, VINNAPAS® 401 continues to form a film at lower temperatures and can be used in the laminating of cold substrates while still maintaining adhesion and heat resistance.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density
  • Solids Content
  • pH
  • Viscosity, dynamic
  • Glass Transition Temp, Tg
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.