MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ex-Tech Plastics PerformaTech™ PVC XSD-28 Static Dissipative PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Manufactured in thickness from 10 to 60 mils, PerformTech XSD-28 is available in rigid vinyl or PET. XSD-28 is a static dissipative sheet engineered specifically for ESD sensitive packaging for use in ESD controlled environments.

Characteristics:
Engineered for packaging to contain ESD-sensitive items and for use in ESD controlled environments.
Static Dissipative range 1 x 105 ohms per square to less than 1 x 1012 ohms per square.
Thickness ranging from .010 to .060”

End Uses:
Thermoformed containers.
High level of surface resistance and volume resistivity is ideal for the containment, transport and long-term storage of ICs, printed circuit boards and other ESD-sensitive components.

Information provided by Ex-Tech Plastics Inc.

Vendors:
Available Properties
  • Density, ASTM D792
  • Tensile Strength, ASTM D882
  • Elongation at Break, ASTM D882
  • Izod Impact, Notched, SOP-MEC-002.01
  • Surface Resistance, EOS/ESD S11.11-1993
  • Surface Resistivity per Square, ASTM D257, 12% Humidity
  • Static Decay, EIA 541
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648-96
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.