MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
GEHR Plastics PPE Polyphenylene Ether  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: Polyphenylenether belongs to the group of amorphous materials and can be used in temperatures ranging from -50°C to approximately 105°C. PPE exhibits a high impact strength, a low water absorption, a very high dimensional stability and a very low tendency to creep. The electrical properties will not be influenced by the surrounding frequencies and therefore can be used in a lot of applications in electrical engineering

Properties

  • high dimensional stability
  • low tendency to creep
  • high thermostability
  • high impact strength
  • good electrical characteristics over a wide frequency range
  • high resistance to hydrolysis
  • self-extinguishing
  • not resistant to some hydrocarbons
Applications include parts for electrical engineering and household utensils, shafts, gear wheels, and parts in the hydrolysis.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Water Absorption at Saturation, ISO 62
  • Hardness, Shore D, DIN 53505
  • Ball Indentation Hardness, ISO 2039-1
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Flexural Strength, ISO 178
  • Charpy Impact, Notched, ISO 179
  • Coefficient of Friction, DIN 53375
  • Volume Resistivity, VDE 0303
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength, VDE 0303
  • Dielectric Loss Index, DIN 53483
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, DIN 53752
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Vicat Softening Point, ISO 306, VST/B/50
  • Minimum Service Temperature, Air
  • Flammability, UL94, UL 94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
GEHR Plastics Inc

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.