MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Lanxess LEWATIT® AF 5 Separations Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® AF 5 is a microporous carbonaceous bead type material designed for downstream process separation and purification. The material is derived from a synthetic polymer, and its adsorptive characteristics are defined by a proprietary conditioning process. This conditioning process provides a unique adsorptive surface with excellent selectivity for small polar molecules from polar solvents. In addition, the narrow and uniform small pores provide some size exclusion chromatographic effects. Lewatit AF 5 is particularly suitable for the following applications:
  • Water treatment (removal of trace organic substances, such as chlorinated hydrocarbons, MTBE, organic phosphates, amines, pesticides and other metabolites)
  • Cleaning of chemical products
  • Removal of organics from electroplating process streams
  • Isolation of active pharmaceutical ingredients
  • Removal of acetic acid from brine
In contrast to activated carbon, the Lewatit AF 5 can be cleaned as often as desired by selecting a suitable regenerant without the need for any additional reactivation. Lewatit AF 5 is remarkable for its well defined uniform pore distribution, high surface area, and high adsorptive capacity. The separation mechanism is partially via low energy hydrogen bonding, resulting in simple elution methods with a variety of solvent. Lewatit AF 5 is commonly eluted with steam, or hot water, without damage to the surface structure of Lewatit AF 5. In contrast to conventional granular carbon adsorbers, Lewatit AF 5 has a narrow bead size distribution, and excellent mechanical stability (mechanical crush strength is approx. 3000 gms/bead in Chatillion measurement). Lewatit AF 5 is ideal for use in fixed bed for fluidized adsorption beds, with no carry-out of fine particles resulting from bead attrition. Lanxess recommends that preliminary tests be carried out at laboratory scale prior to industrial application. The laboratory experiments should define the optimum loading and elution conditions to maximize capacity, and elution techniques to recover the surface area for subsequent loading cycles.

Information provided by Lanxess.

Vendors:
Available Properties
  • Bulk Density
  • Density
  • Bead Size, >90%
  • Storage Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lanxess, Spinoff of Bayer

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.