| MP531107M is a high performance UV curing adhesive engineered to bond a wide range of plastic, metals, and glass. It can be used in a variety of product assemblies and it promotes innovative design solutions. Our MP531107M has passed ISO 10993 Cytotoxicity testing and it is a leading performer when used for medical device applications. This maximum performance adhesive is tack free and creates an extremely strong, durable bond. During in-line inspection this adhesive fluoresces a blue color when using a low intensity black light. This UV adhesive Is a fast curing low viscosity product. MP531107M is often cured with an electroless lamp D, medium pressure metal halide lamp. This UV adhesive also works well with UV light emitted diodes (UV LED) at wavelengths of 365 nm to 410 nm. Design engineers select MP531107M for the optimum in finished product quality, reliability, performance, and cost effectiveness. MP531107M is an essential tool in improving overall product quality, lowering per unit cost, and reducing processing time. Benefits: Superior Bond Strength, Solvent Free, Low Odor, Improves Finished Product Quality, Durable, Good Impact and Vibration Resistance, Easily Automated, No Clean Up. Substrate Applications: Polycarbonate (PC) Polyvinylchloride (PVC), Polyethylene, Polypropylene requires surface treatment such as corona, etc., Glass, Metal.Information provided by Adhesive Systems, Inc. |