MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes: Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhesive characteristics are designated by exceptionally high shear and peel strengths on a variety of substrates. This film adhesive is designed for both solid panel and honeycomb constructions. The film adhesive was designed to meet the specifications of MMM-A132B Type I Class 2. Aroply™ contains an optimum level of carbon nanotubes for additional toughness and enhanced mechanical properties. The carbon nanotubes use molecular dispersion technology to ensure enhancements are evenly distributed throughout the adhesive.

Features:

  • Wide range of cure properties: 180°F-350°F (82°C-177°C) at vacuum or clamp pressure to >100 psi
  • Tacky for adherence to desired location
  • Long Open Time: 30+ days in standard shop conditions
  • Adaptable to many processes

Vendors:
Available Properties
  • Flexural Strength, 5 lb Core, 6 hrs @ 220°F, Vacuum Bag
  • Flexural Strength, 8 lb Core, 6 hrs @ 220°F, Vacuum Bag
  • Flexural Modulus, 5 lb Core, 6 hrs @ 220°F, Vacuum Bag
  • Flexural Modulus, 8 lb Core, 6 hrs @ 220°F, Vacuum Bag
  • Shear Strength, ASTM D1002, Cure Cycle, 2 hrs @ 250°F, FPL Acid Etched 6061-T6, Std Dev 94
  • Shear Strength, ASTM D1002, Cure Cycle, 4 hrs @ 220°F, FPL Acid Etched 6061-T6, Std Dev 132
  • Shear Strength, ASTM D1002, Cure Cycle, 8 hrs @ 180°F, FPL Acid Etched 6061-T6, Std Dev 158
  • Shear Strength, ASTM D1002, Cure Cycle, 2 hrs @ 250°F, FPL Acid Etched 6061-T6, Std Dev 64
  • Shear Strength, ASTM D1002, Cure Cycle, 4 hrs @ 220°F, FPL Acid Etched 6061-T6, Std Dev 72
  • Shear Strength, ASTM D1002, Cure Cycle, 8 hrs @ 180°F, FPL Acid Etched 6061-T6, Std Dev 144
  • Shear Strength, ASTM D1002, Cure Cycle, 8 hrs @ 180°F, FPL Acid Etched 6061-T6, Std Dev 502
  • Shear Strength, ASTM D1002, Cure Cycle, 2 hrs @ 250°F, FPL Acid Etched 6061-T6, Std Dev 470
  • Shear Strength, ASTM D1002, Cure Cycle, 6 hrs @ 200°F, FPL Acid Etched 6061-T6, Std Dev 100
  • Shear Strength, ASTM D1002, Cure Cycle, 2 hrs @ 250°F, FPL Acid Etched 6061-T6, Std Dev 121
  • Shear Strength, 2 hrs @ 250°F, Metal Clamp Pressure, 6061 T6 FPL Etched
  • Shear Strength, ASTM D1002, Cure Cycle, 1 hr @ 250°F, FPL Acid Etched 6061-T6, Std Dev 456
  • Shear Strength, ASTM D1002, Cure Cycle, 6 hrs @ 200°F, FPL Acid Etched 6061-T6, Std Dev 150
  • Shear Strength, ASTM D1002, Cure Cycle, 2 hrs @ 250°F, FPL Acid Etched 6061-T6, Std Dev 138
  • Shear Strength, ASTM D1002, Cure Cycle, 6 hrs @ 200°F, FPL Acid Etched 6061-T6, Std Dev 109
  • Shear Strength, ASTM D1002, Cure Cycle, 2 hrs @ 250°F, FPL Acid Etched 6061-T6, Std Dev 117
  • Shear Strength, ASTM D1002, Cure Cycle, 2 hrs @ 250°F, FPL Acid Etched 6061-T6, Std Dev 218
  • Shear Strength, ASTM D1002, Cure Cycle, 4 hrs @ 220°F, FPL Acid Etched 6061-T6, Std Dev 128
  • Shear Strength, ASTM D1002, Cure Cycle, 6 hrs @ 220°F, FPL Acid Etched 6061-T6, Std Dev 134
  • Shear Strength, ASTM D1002, Cure Cycle, 1 hr @ 250°F, FPL Acid Etched 6061-T6, Std Dev 9
  • Shear Strength, ASTM D1002, Cure Cycle, 2 hrs @ 250°F, FPL Acid Etched 6061-T6, Std Dev 128
  • Shear Strength, ASTM D1002, Cure Cycle, 90 min @ 250°F, FPL Acid Etched 6061-T6, Std Dev 84
  • Shear Strength, 2 hrs @ 250°F, Metal Clamp Pressure, 6061 T6 FPL Etched
  • Shear Strength, ASTM D1002, Cure Cycle, 90 min @ 250°F, FPL Acid Etched 6061-T6, Std Dev 96
  • Peel Strength, ASTM D1876, T-Peel, Cure Cycle, 1 hr @ 250°F, FPL Acid Etched 6061-T6, Std Dev 1.6
  • Peel Strength, ASTM D1876, T-Peel, Cure Cycle, 6 hrs @ 220°F, FPL Acid Etched 6061-T6, Std Dev 1.9
  • Peel Strength, ASTM D1876, T-Peel, Cure Cycle, 90 min @ 250°F, FPL Acid Etched 6061-T6, Std Dev 2.3
  • Peel Strength, ASTM D1876, T-Peel, Cure Cycle, 90 min @ 250°F, FPL Acid Etched 6061-T6, Std Dev 3.1
  • Peel Strength, ASTM D1876, T-Peel, Cure Cycle, 2 hrs @ 250°F, FPL Acid Etched 6061-T6, Std Dev 3.4
  • Peel Strength, T-Peel, 2 hrs @ 250°F, Metal Clamp Pressure, 6061 T6 FPL Etched
  • Peel Strength, T-Peel, 2 hrs @ 250°F, Metal Clamp Pressure, 6061 T6 FPL Etched
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Zyvex Performance Materials (ZPM)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.