MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Megaflow® AW Ultra-Clean Hydraulic Oil ISO Grade 100
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Megaflow AW Ultra-Clean Hydraulic Oil is a high-quality antiwear hydraulic oil developed for use in industrial and mobile hydraulic systems that require an oil with a high level of fluid cleanliness. It provides the same performance benefits as Megaflow® AW Hydraulic Oil, plus it is filtered to a typical ISO Cleanliness Code of 17/15/11 for use in hydraulic systems with tight tolerances where particle contamination can cause operational problems. Megaflow AW Ultra-Clean Hydraulic Oil is formulated to provide excellent wear protection for hydraulic pumps and motors, and to protect hydraulic system components against rust and corrosion. It has excellent oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It has excellent water-separating properties to minimize the formation of emulsions, and is resistant to excessive foam buildup that can cause poor or sluggish hydraulic system response. Megaflow AW Ultra-Clean Hydraulic Oil meets the performance requirements of all major hydraulic pump manufacturers, and is recommended for use in all types of high-pressure, high-speed hydraulic pumps.

Applications:

  • Hydraulic systems on industrial, mobile and marine equipment, especially where particle contamination can cause operational problems
  • Automated machine tools
  • Hydraulic elevators, hoists, presses and floor jacks
  • Marine cargo winches and steering systems
  • Service station lifts
  • Air tools and other pneumatic equipment lubricated through air line lubricators
  • Chain drives
  • Electric motor bearings
Megaflow AW Ultra-Clean Hydraulic Oil meets the requirements of the following industry and OEM specifications:
  • Bosch Rexroth RE 90220, Type HLP
  • DIN 51524 Part 2, Antiwear Hydraulic Oils, Type HLP
  • Eaton-Vickers I-286-S, M-2950-S
  • German Steel Industry SEB 181222
  • ISO 11158:1997, Family H (Hydraulic Systems), Type HM
  • Parker Hannifin (Denison) HF-0, HF-1, HF-2
  • U.S. Steel 127
Features/Benefits
  • Excellent wear protection for hydraulic pumps and motors
  • Reliable operation of hydraulic valves and actuators
  • Excellent oxidation resistance and thermal stability
  • Protects against rust and corrosion
  • Excellent water-separating properties
  • Good foam resistance
  • Good low-temperature properties for cold start-ups
  • Meets ISO Cleanliness Code rating of 17/15/11

    Information provided by Phillips 66 Lubricants.

  • Vendors:
    Available Properties
    • Specific Gravity
    • Density
    • Viscosity Measurement, Index
    • Saybolt Viscosity at 100°F
    • Saybolt Viscosity at 210°F
    • Kinematic Viscosity at 40°C (104°F)
    • Kinematic Viscosity at 100°C (212°F)
    • Oxidative Stability, ASTM D2272, RPVOT
    • Oxidative Stability, ASTM D943-04a, TOST
    • ASTM Color, ASTM D1500
    • Total Acid Number, ASTM D974, [mg KOH/g]
    • Dielectric Strength, ASTM D877
    • Pour Point
    • Flash Point, COC
    • Zinc, Zn
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    none

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.