MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AURUM JCF3030 offers a unique balance of mechanical, thermal, and tribological properties for outstanding performance in demanding automotive, business machinery, industrial equipment, aerospace, and semiconductor equipment applications. AURUM components offer excellent mechanical strength and toughness, dimensional stability, low outgassing, and exceptional radiation resistance. In addition, AURUM exhibits outstanding resistance to hydraulic, automotive, and many industrial fluids and solvents, a low coefficient of thermal expansion, creep resistance, and flame retardancy. AURUM JCF3030 withstands high PV levels and provides a low wear factor and low friction surface over a broad temperature range in lubricated environments.

Applications: AURUM JCF3030 components are excellent replacements for metals, ceramics, and other plastics. High performance AURUM parts include: thrust washers and oil seal rings for automotive and off road vehicle transmissions, thermal insulators and stripper fingers for high-speed copiers, jet engine components, check valve balls, spline couplings, heat-resistant gears, vanes, wear strips, and valve seats. Other AURUM applications include carriers for aluminum hard disks and silicon wafers, journal bearings, and bearing retainers.

Information provided by DuPont

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570, 24 hrs @ 73°F
  • Moisture Absorption at Equilibrium, 73°F; 60 RH, 24hrs
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Melt Flow, ASTM D1238
  • Melt Flow, ASTM D1238
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Yield, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Melting Point, DSC
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Glass Transition Temp, Tg, DSC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Mitsui Chemicals America

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.