MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SABIC SABIC® LLDPE 218WJ PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: 218WJ is a butene Linear Low Density Polyethylene TNPP free grade suitable for general-purpose packaging. It is easy to process giving good tensile properties, impact strength and optical properties. 218WJ contains slip and antiblock additives.

Information provided by SABIC

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ASTM D1238
  • Film Tensile Strength at Yield, MD, ASTM D882, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • Film Tensile Strength at Yield, TD, ASTM D882, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • Film Elongation at Break, MD, ASTM D882, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • Film Elongation at Break, TD, ASTM D882, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • Puncture Energy, SABIC method, J/m
  • Elmendorf Tear Strength MD, ASTM D1922, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • Elmendorf Tear Strength TD, ASTM D1922, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • Dart Drop, ASTM D1709, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • Film Tensile Strength at Break, MD, ASTM D882, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • Film Tensile Strength at Break, TD, ASTM D882, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • 1% Secant Modulus, MD, ASTM D882, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • 1% Secant Modulus, TD, ASTM D882, Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  • Vicat Softening Point, ASTM D1525
  • Haze, ASTM D1003, 2.5 BUR using 100% 218NJ.
  • Gloss, ASTM D2457, 60°; Mechanical properties have been measured by producing 30 µ film with 2.5 BUR using 100% 218NJ.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.