MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Mitsubishi PVA Polyvinyl Alcohol, Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: PVA filament is quickly soluble in water, bonds well to plastics, and prints easily. Therefore, it is an excellent supporting material for dual extruder 3D printing. This polyvinyl alcohol-based filament is nontoxic, and biodegradable once dissolved in water. PVA is also available in colors and has a high tensile strength for applications other then supporting material.

Features:

  • Excellent water solubility
  • Easy to print at low temperature
  • Good bonding to various plastics such as PLA
  • Biodegradable when dissolved in water
  • Limited smell
Colors: PVA is available from stock in its natural color. For specific applications, PVA is available in colors on request

Information provided by Mitsubishi Chemical.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Filament Diameter, Tolerance: 50 µm, =95% Roundness
  • Filament Diameter, Tolerance: 100 µm, =95% Roundness
  • Melt Flow, ISO 1133
  • Storage Temperature
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Tensile Modulus, ISO 527, (E)
  • Charpy Impact, Notched, ISO 179
  • Melting Point
  • Vicat Softening Point, ISO 306 A10
  • Processing Temperature, Printing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.