  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Go Yen Chemical GY-FR-B59 GYC Synthetic Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Outstanding flame retardancy; Long term life time; Well Compatibility; High Stability; Non-toxic and odorless; Do not contain heavy metals

Applications:

  • Various kinds of thermoplastics and thermosetting plastics such as ABS, HIPS, PE, phenolic resin, unsaturated resin, polyurethane foam adhesive, polycarbonates and high impact polystyrene
  • Cellulose acetate, cellulose nitrate, PC/ABS, PPO/HIPS
  • Different kinds of synthetic and nature rubber
  • Modified PPO and various engineering plastic
  • Highly effective when reacted into epoxy resin systems
  • Films, paint, coating, lacquers, molding powders and other flame retard applications.
Advantages:
  • Offer great flame retardancy by high thermal stability
  • Improved processing properties
  • Increased physical property performance
  • Can provide strong thermal decomposition
  • Can be flame-resistant for a long time (durability)
  • Do not generate migration when application
  • Can be well compatible with multi-kinds polymers & resins

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • Melting Point
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.