| SMC 3300 RF R33 is a sheet molding compound based on an unsaturated polyester resin, fire retardant grade, halogen-free, reinforced with glass fibers. This SMC has been developed for electrical application. SMC 3300 RF R33 joint excellent mechanical properties and good fire protection grade. SMC 3300 RF R33 is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.Information provided by Polynt Composites. |