MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Syensqo (Solvay Specialty Polymers) Torlon® 7130 PAI, 30% carbon fiber
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: 30% carbon fiber, best stiffness, best retention of stiffness at high temperatures, best fatigue resistance, electrically conductive

Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal expansion characteristics similar to steel, and therefore excellent dimensional stability.

Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep, and chemicals.

The potential applications for this resin include metal replacement, sliding vanes, aerospace parts, impellors, shrouds, pistons, and housings.

It is available in injection molding and extrusion (E) grades.

Markets/Uses: Aircraft / Mechanical & Structural Applications / Brackets and Hinges; Aircraft / Mechanical & Structural Applications / Engine Components; Aircraft / Mechanical & Structural Applications / Engine Fan Cowling Vents; Aircraft / Mechanical & Structural Applications / Fan Impeller; Aircraft / Mechanical & Structural Applications / Mounting Support Rails; Aircraft / Mechanical & Structural Applications / Seals; Aircraft / Mechanical & Structural Applications / Stock Shapes for Prototyping; Aircraft / Mechanical & Structural Applications / Support Brackets; Automotive / Mechanical & Structural Parts / Gears; Films / High Temperature Films / Brackets and Hinges; Films / High Temperature Films / Engine Components; Films / High Temperature Films / Engine Fan Cowling Vents; Films / High Temperature Films / Fan Impeller; Films / High Temperature Films / Mounting Support Rails; Films / High Temperature Films / Seals; Films / High Temperature Films / Stock Shapes for Prototyping; Miscellaneous / Industrial / Compressor Components; Oil & Gas / Down Hole / Back-Up Seal Rings; Oil & Gas / Down Hole / Compressor Components; Oil & Gas / Down Hole / Down Hole Connectors; Oil & Gas / Down Hole / Electrical Connectors; Oil & Gas / Down Hole / Motor End Plate; Oil & Gas / Down Hole / Poppets; Semiconductor / Fabrication & Testing / Mechanical Fasteners

Applications: Aerospace Applications; Aircraft Applications; Business Equipment; Connectors; Electrical/Electronic Applications; Film; Gears; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Oil/Gas Applications; Semiconductor Molding Compounds

Features: Chemical Resistant; Creep Resistant; Fatigue Resistant; Flame Retardant; Good Compressive Strength; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Temperature Strength; Semi Conductive

Injection notes: Minimum drying conditions: 3 hours at 350°F (177°C), 4 hours at 300°F (149°C), or 16 hours at 250°F (121°C).
Compression Ratio: 1:1 to 1.5:1
Begin hold pressure at a high setting 6,000-8,000 psi (41.37-55.16 MPa), for several seconds, then drop off to 3,000-5,000 psi (20.69-34.48 MPa), for the duration of the hold pressure sequence.
Molded parts must be post cured.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Tensile Strength, ASTM D638
  • Tensile Stress, ASTM D1708
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Rear Barrel Temperature
  • Nozzle Temperature
  • Mold Temperature
  • Drying Temperature
  • Moisture Content, Injection
  • Back Pressure
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.