MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Assab Steels DF-3 Cold Work Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Oil-Hardening Steel

Material Notes: DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:
  • Good machinability
  • Good dimensional stability in hardening
  • A good combination of high surface hardness and toughness after hardening and tempering.

These characteristics combine to give a steel suitable for the manufacture of tooling with good tool-life and high production economy.

DF-3 can be supplied in various finishes including hot-rolled, pre-machined, fine-machined and precision ground. It is also available in the form of hollow bar.

AISI 01

Vendors:
Available Properties
  • Density
  • Density
  • Density
  • Hardness, Rockwell C, 790°C Austenitizing temperature, for tempering at 550°C
  • Hardness, Rockwell C, 820°C Austenitizing temperature, for tempering at 550°C
  • Hardness, Rockwell C, 790°C Austenitizing temperature, for tempering at 250°C
  • Hardness, Rockwell C, 820°C Austenitizing temperature, for tempering at 250°C
  • Hardness, Rockwell C, Hardened and tempered.
  • Hardness, Rockwell C, 780°C hardening temp
  • Hardness, Rockwell C, At 860°C hardening temp
  • Hardness, Rockwell C, 820°C hardening temp
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Compressive Strength, HRC 45 Rc0.2
  • Compressive Strength, HRC 45 Rcm
  • Compressive Strength, HRC 55 Rc0.2
  • Compressive Strength, HRC 62 Rc0.2
  • Compressive Strength, HRC 55 Rcm
  • Compressive Strength, HRC 62 Rcm
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Tungsten, W
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.