| Description: Krasol® LBH 2000 is a linear, low molecular weight, polybutadiene polymer. The polymer is terminated with secondary hydroxyl groups with a hydroxyl functionality of 1.95. The resin is liquid at room temperature and is miscible in non-polar organic liquids, oils, and bitumens. Product Highlights / Performance Properties: - Good electrical insulative properties
- Good low temperature flexibility
- Narrow molecular weight distribution
- Hydrolytically stable
- Forms stable prepolymers
Suggested Applications: - Prepolymers
- Thermoplastic elastomers
- Adhesives and sealants
- Coatings
- Electrical potting and encapsulation
- Polymer modification
- Polyurethanes
Information provided by Cray Valley |