MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Akrochem 237 Silicone Emulsions
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: SEM Series silicone emulsions are carefully formulated emulsions of dimethyl, alkyl modified dimethyl or a reactive silicone fluid and water. They are primarily designed for use in applications for rubber and plastic release agents, furniture polish, cosmetic, textile finishing and other specialty formulations. Each emulsion is based upon a silicone fluid of different viscosity ranging from 100 to >100,000 centistokes. Most SEM silicone emulsions have a specific gravity of approximately 1.00, a freeze/thaw stability of 4 cycles minimum and are white in color, except SEM401, which is yellowtinted white. SEM silicone emulsions contain a corrosion inhibitor and an anti-fungicide.

Applications: In mold release application, SEM Silicone Emulsions are normally diluted with water to 0.5% to 2.5% active silicone to be sprayed, dipped or brushed on a mold. However, in a polish or specialty product formulation, the emulsions are normally used in their concentrated form. In most release applications a low-pressure spray gives the best results. Depending on the material being released, one application per cycle or one application per multiple cycles may be needed.

Information provided by Akrochem Corporation

Vendors:
Available Properties
  • pH
  • Viscosity Measure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.