MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
COMSOL BASICS
Overview of materials for Thermoplastic Polyimide, Unfilled
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Unfilled

Vendors:
Available Properties
  • Density, Average value: 1.42 g/cc Grade Count:16
  • Water Absorption, Average value: 0.620 % Grade Count:9
  • Water Absorption, Average value: 0.300 % Grade Count:1
  • Water Absorption, Average value: 0.300 % Grade Count:1
  • Moisture Absorption at Equilibrium, Average value: 0.695 % Grade Count:4
  • Linear Mold Shrinkage, Average value: 0.00940 cm/cm Grade Count:4
  • Hardness, Shore D, Average value: 84.0 Grade Count:7
  • Tensile Strength, Ultimate, Average value: 93.1 MPa Grade Count:15
  • Tensile Strength, Ultimate, Average value: 61.5 MPa Grade Count:4
  • Tensile Strength, Yield, Average value: 57.9 MPa Grade Count:1
  • Elongation at Break, Average value: 26.7 % Grade Count:13
  • Elongation at Break, Average value: 34.3 % Grade Count:3
  • Elongation at Yield, Average value: 90.0 % Grade Count:1
  • Modulus of Elasticity, Average value: 3.90 GPa Grade Count:7
  • Flexural Yield Strength, Average value: 124 MPa Grade Count:12
  • Flexural Yield Strength, Average value: 114 MPa Grade Count:3
  • Flexural Modulus, Average value: 5.86 GPa Grade Count:12
  • Flexural Modulus, Average value: 11.8 GPa Grade Count:3
  • Compressive Strain at Break, Average value: 42.3 % Grade Count:3
  • Compressive Yield Strength, Average value: 161 MPa Grade Count:7
  • Compressive Yield Strength, Average value: 76.5 MPa Grade Count:2
  • Compressive Modulus, Average value: 2.95 GPa Grade Count:4
  • Fatigue Strength, Average value: 21.4 MPa Grade Count:1
  • Fatigue Strength, Average value: 21.4 MPa Grade Count:1
  • Shear Strength, Average value: 78.5 MPa Grade Count:1
  • Izod Impact, Notched, Average value: 0.760 J/cm Grade Count:6
  • Charpy Impact Unnotched, Average value: 2.52 J/cm² Grade Count:4
  • Charpy Impact, Notched, Average value: 0.203 J/cm² Grade Count:3
  • Coefficient of Friction, Average value: 0.352 Grade Count:4
  • Electrical Resistivity, Average value: 2.96e+17 ohm-cm Grade Count:8
  • Surface Resistance, Average value: 2.23e+17 ohm Grade Count:5
  • Dielectric Constant, Average value: 3.38 Grade Count:6
  • Dielectric Strength, Average value: 112 kV/mm Grade Count:5
  • Dissipation Factor, Average value: 0.00234 Grade Count:4
  • CTE, linear, Average value: 44.6 µm/m-°C Grade Count:5
  • CTE, linear, Average value: 55.3 µm/m-°C Grade Count:9
  • CTE, linear, Transverse to Flow, Average value: 55.0 µm/m-°C Grade Count:1
  • Specific Heat Capacity, Average value: 1.07 J/g-°C Grade Count:7
  • Specific Heat Capacity, Average value: 1.21 J/g-°C Grade Count:2
  • Thermal Conductivity, Average value: 0.286 W/m-K Grade Count:6
  • Thermal Conductivity, Average value: 0.250 W/m-K Grade Count:2
  • Maximum Service Temperature, Air, Average value: 248 °C Grade Count:5
  • Deflection Temperature at 1.8 MPa (264 psi), Average value: 346 °C Grade Count:4
  • Glass Transition Temp, Tg, Average value: 189 °C Grade Count:7
  • Decomposition Temperature, Average value: 502 °C Grade Count:3
  • Flammability, UL94, Grade Count:9
  • Oxygen Index, Average value: 50.0 % Grade Count:4
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.