| Available Properties |
|---|
- Density, ISO 1183
- Melt Density
- Water Absorption, Sim. to ISO 62
- Moisture Absorption, Sim. to ISO 62
- Viscosity Number, ISO 307, 1157, 1628
- Linear Mold Shrinkage, Flow, ISO 294-4, 2577
- Linear Mold Shrinkage, Flow, ISO 294-4, Postmolding shrinkage
- Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
- Linear Mold Shrinkage, Transverse, ISO 294-4, Postmolding shrinkage
- Melt Flow, ISO 1133, cm³/10min Volumetric
- Melt Flow, ISO 1133
- Tensile Strength at Break, ISO 527-1/-2
- Elongation at Break, ISO 527-1/-2
- Tensile Modulus, ISO 527-1/-2
- Flexural Strength, ISO 178
- Flexural Modulus, ISO 178
- Poissons Ratio
- Shear Strength, ASTM D 732
- Izod Impact, Notched (ISO), ISO 180/1A
- Izod Impact, Notched (ISO), ISO 180/1A
- Izod Impact, Notched (ISO), ISO 180/1A
- Izod Impact, Unnotched (ISO), ISO 180/1U
- Izod Impact, Unnotched (ISO), ISO 180/1U
- Izod Impact, Unnotched (ISO), ISO 180/1U
- Charpy Impact Unnotched, ISO 179/1eU
- Charpy Impact Unnotched, ISO 179/1eU
- Charpy Impact Unnotched, ISO 179/1eU
- Charpy Impact, Notched, ISO 179/1eA
- Charpy Impact, Notched, ISO 179/1eA
- Charpy Impact, Notched, ISO 179/1eA
- Tensile Creep Modulus, 1 hour, ISO 899-1, 1h
- Tensile Creep Modulus, 1000 hours, ISO 899-1, 1000h
- Volume Resistivity, IEC 62631-3-1
- Surface Resistance, IEC 62631-3-2
- Dielectric Constant, IEC 62631-2-1
- Dielectric Constant, IEC 62631-2-1
- Dielectric Strength, IEC 60243-1
- Dissipation Factor, IEC 62631-2-1
- Dissipation Factor, IEC 62631-2-1
- Comparative Tracking Index, IEC 60112
- CTE, linear, Parallel to Flow, ISO 11359-1/-2
- CTE, linear, Transverse to Flow, ISO 11359-1/-2
- Specific Heat Capacity, Melt
- Thermal Conductivity, Melt
- Melting Point, ISO 11357-1/-3, 10°C/min
- Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
- Vicat Softening Point, ISO 306, 50°C/h, 50N
- Glass Transition Temp, Tg, ISO 11357-1/-2, 10°C/min
- Flammability, UL94, IEC 60695-11-10
- Flammability, UL94, IEC 60695-11-10
- Flame Spread, ISO 3795 (FMVSS 302)
- Oxygen Index, ISO 4589-1/-2
- Glow Wire Ignition Temperature, IEC 60695-2-13
- Glow Wire Ignition Temperature, IEC 60695-2-13
- Glow Wire Ignition Temperature, IEC 60695-2-13
- Glow Wire Ignition Temperature, IEC 60695-2-13
- Glow Wire Ignition Temperature, IEC 60695-2-13
- Melt Temperature, Optimum, Injection
- Melt Temperature, Range, Injection
- Mold Temperature, Optimum, Injection
- Mold Temperature, Injection
- Ejection Temperature, Injection
- Drying Temperature, Injection
- Dry Time, Injection, Dehumidified Dryer
- Moisture Content, Injection
- Hold Pressure, Injection
|
| | |