MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Rotational Molded

Material Notes: Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excellent mechanical and environmental resistance properties. Available as black powder.

Applications: High quality Polyethylene recommended for producing industrial tanks, cisterns, agricultural tanks, chemical tanks or for applications requiring excellent chemical resistance, impact strength and ESCR resistance. Molded parts have a smooth surface finish. This product contains mold release internal agents which eliminate the application of mold release products in the mold inner surface.

The carrier of this product meets all FDA requirements as specified in 21 CFR 177.1520 and CONEG (as a compound), covering safe use in articles for direct food contact.

Information provided by Polimeros Mexicanos

Key Words: Recommended for industrial tanks, cisterns, agricultural tanks, chemical tanks, etc.
Vendors:
Available Properties
  • Density, ASTM D1505
  • ESCR 100% Igepal®, ASTM D1693
  • ESCR 10% Igepal®, ASTM D1693
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D638, 2 in/min
  • Tensile Strength, Yield, ASTM D638, 2 in/min
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Flexural Modulus, 1% Secant, ASTM D790
  • Impact Test, ARM STD test, 0.125 in.
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.