MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Lord Adhesives Chemlok® 320/310-B Black Epoxy, 320 Resin Adhesive System
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD Chemlok® 320/310-B Black adhesive is a two-component epoxy adhesive system used to bond cured rubber treated with Chemlok 7701 surface treatment. This adhesive system also bonds metals and plastics, both thermosets and thermoplastics.

Features: rapidly cures when heated at 93-162°C (200-325°F). provides good impact resistance down to -40°C (-40°F). contains no solvent, nonflammable and virtually odorless. resists humidity, salt spray and temperature extremes. resists postbakes up to 204°C (400°F). solvent resistant when cured; anti-corrosion processes including phosphatizing and ELPO (e-coat) coatings do not affect the adhesive or its bond strength.

All information provided by Lord.

Vendors:
Available Properties
  • Density
  • Solids Content, by weight
  • Brookfield Viscosity, Brookfield HBF, Helipath, 5 rpm
  • Minimum Service Temperature, Air
  • Flash Point, Seta
  • Shelf Life, from shipment date in original, unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.