| Crossvinil: is the trade name of our PVC compounds. CrossvinilEK/2 AZC: the polyvinyl chloride compound, plasticized and stabilized with Ca-Zn. Flame Retardant type. This compound meets Dir. 2002/95/CE (RoHS) Certify: IEC 60502 ST2 90°C,IEC 60332-3-22 Cat A Information provided by Crosspolimeri S.P.A. |