| Available Properties |
|---|
- Specific Gravity
- Hardness, Shore A
- Hardness, Shore A, Concentrated Nitric Acid
- Hardness, Shore A, 50% MeOH/50% FUEL C
- Hardness, Shore A, 50% MeOH/50% FUEL C
- Hardness, Shore A, 50% MeOH/50% FUEL C
- Hardness, Shore A, 15% EtOH/85% FUEL C
- Hardness, Shore A, 50% MeOH/50% FUEL C
- Hardness, Shore A, 15% EtOH/85% FUEL C
- Hardness, Shore A, Stauffer Blend 7700
- Hardness, Shore A, 15% EtOH/85% FUEL C
- Hardness, Shore A, Methanol
- Hardness, Shore A, 85% EtOH/15% FUEL C
- Hardness, Shore A, Methanol
- Hardness, Shore A, Methanol
- Hardness, Shore A, 85% EtOH/15% FUEL C
- Hardness, Shore A, 85% EtOH/15% FUEL C
- Hardness, Shore A, Service Fluid 101
- Hardness, Shore A, Ethanol
- Hardness, Shore A, Methanol
- Hardness, Shore A, 15% EtOH/85% FUEL C
- Hardness, Shore A, Concentrated Nitric Acid
- Hardness, Shore A, ASTM Oil #1 (IRM 901)
- Hardness, Shore A, Sodium Hypochlorite
- Hardness, Shore A, Ethanol
- Hardness, Shore A, 85% EtOH/15% FUEL C
- Hardness, Shore A, Hydrochloric Acid 37%
- Hardness, Shore A, Hydrochloric Acid 37%
- Hardness, Shore A, Ethanol
- Hardness, Shore A, ASTM Oil #3 (IRM 903)
- Hardness, Shore A, Ethanol
- Hardness, Shore A, Sodium Hydroxide (50%)
- Hardness, Shore A, Sodium Hydroxide (50%)
- Hardness, Shore A, Hydrochloric Acid 37%
- Hardness, Shore A, Concentrated Nitric Acid
- Hardness, Shore A, Sodium Hypochlorite
- Hardness, Shore A, ASTM Reference Fuel C
- Hardness, Shore A, Concentrated Sulfuric Acid
- Hardness, Shore A, Concentrated Sulfuric Acid
- Hardness, Shore A, Concentrated Sulfuric Acid
- Hardness, Shore A, Sodium Hypochlorite
- Hardness, Shore A, Heat Aged
- Hardness, Shore A, Heat Aged
- Hardness, Shore A, ASTM Reference Fuel A
- Hardness, Shore A, Sodium Hydroxide (50%)
- Tensile Strength
- Tensile Strength, Hydrochloric Acid 37%
- Tensile Strength, Concentrated Sulfuric Acid
- Tensile Strength, ASTM Reference Fuel A
- Tensile Strength, ASTM Reference Fuel C
- Tensile Strength, Stauffer Blend 7700
- Tensile Strength, Service Fluid 101
- Tensile Strength, Concentrated Sulfuric Acid
- Tensile Strength, Sodium Hypochlorite
- Tensile Strength, ASTM Oil #3 (IRM 903)
- Tensile Strength, Concentrated Nitric Acid
- Tensile Strength, ASTM Oil #1 (IRM 901)
- Tensile Strength, Sodium Hydroxide (50%)
- Tensile Strength, Heat Aged
- Tensile Strength, Heat Aged
- Elongation, Ultimate
- Elongation, Ultimate, ASTM Reference Fuel A
- Elongation, Ultimate, Sodium Hypochlorite
- Elongation, Ultimate, ASTM Oil #1 (IRM 901)
- Elongation, Ultimate, ASTM Reference Fuel C
- Elongation, Ultimate, Hydrochloric Acid 37%
- Elongation, Ultimate, ASTM Oil #3 (IRM 903)
- Elongation, Ultimate, Sodium Hydroxide (50%)
- Elongation, Ultimate, Stauffer Blend 7700
- Elongation, Ultimate, Concentrated Nitric Acid
- Elongation, Ultimate, Concentrated Sulfuric Acid
- Elongation, Ultimate, Service Fluid 101
- Elongation, Ultimate, Concentrated Sulfuric Acid
- Elongation, Ultimate, Heat Aged
- Elongation, Ultimate, Heat Aged
- 100% Modulus
- Tear Strength, Die B
- Tear Strength, Die C
- Compression Set, Plied
- Compression Set, Plied
- Compression Set, Plied
- Brittleness Temperature
- Shrinkage, Volume, Sodium Hydroxide (50%)
- Shrinkage, Volume, Sodium Hydroxide (50%)
- Shrinkage, Volume, Sodium Hydroxide (50%)
- Shrinkage, Volume, Sodium Hypochlorite
- Shrinkage, Volume, Sodium Hypochlorite
- Shrinkage, Volume, Sodium Hypochlorite
- Shrinkage, Volume, ASTM Reference Fuel A
- Shrinkage, Volume, ASTM Oil #1
- Shrinkage, Volume, Ethanol
- Shrinkage, Volume, Ethanol
- Shrinkage, Volume, 85% EtOH/15% FUEL C
- Shrinkage, Volume, ASTM Reference Fuel C
- Shrinkage, Volume, ASTM Oil #3
- Shrinkage, Volume, Methanol
- Shrinkage, Volume, 85% EtOH/15% FUEL C
- Shrinkage, Volume, Ethanol
- Shrinkage, Volume, Hydrochloric Acid 37%
- Shrinkage, Volume, 15% EtOH/85% FUEL C
- Shrinkage, Volume, Hydrochloric Acid 37%
- Shrinkage, Volume, Concentrated Nitric Acid
- Shrinkage, Volume, Ethanol
- Shrinkage, Volume, Methanol
- Shrinkage, Volume, 85% EtOH/15% FUEL C
- Shrinkage, Volume, Concentrated Sulfuric Acid
- Shrinkage, Volume, Concentrated Sulfuric Acid
- Shrinkage, Volume, 15% EtOH/85% FUEL C
- Shrinkage, Volume, Concentrated Nitric Acid
- Shrinkage, Volume, 50% MeOH/50% FUEL C
- Shrinkage, Volume, Service Fluid 100
- Shrinkage, Volume, Methanol
- Shrinkage, Volume, 85% EtOH/15% FUEL C
- Shrinkage, Volume, Methanol
- Shrinkage, Volume, Stauffer Blend 7700
- Shrinkage, Volume, 50% MeOH/50% FUEL C
- Shrinkage, Volume, Concentrated Sulfuric Acid
- Shrinkage, Volume, 15% EtOH/85% FUEL C
- Shrinkage, Volume, Hydrochloric Acid 37%
- Shrinkage, Volume, 15% EtOH/85% FUEL C
- Shrinkage, Volume, 50% MeOH/50% FUEL C
- Shrinkage, Volume, 50% MeOH/50% FUEL C
- Shrinkage, Volume, Concentrated Nitric Acid
|
| | |