MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Harris Acoustic Sensors EC-31 Barium Titanate Piezoelectric  (discontinued **)
Categories: Ceramic; Oxide; Titanium Oxide; Piezoelectric

Material Notes: This modified barium titanate which combines high voltage sensitivity with good temperature characteristics - 10 to 60°C range. This is a proven material for hydrophones and other receiving devices and low power projectors, ideal for fish-finder applications.

Data provided by Harris Acoustic Sensors. Harris Acoustic Sensors has acquired EDO Ceramics.

Key Words: BaTiO3; Barium Titanium Oxide
Vendors:
Available Properties
  • Density
  • Modulus of Elasticity, Young's Modulus
  • Curie Temperature
  • Dielectric Constant
  • Dissipation Factor, low field
  • Piezoelectric Longitudinal Coupling Factor, k33
  • Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V, strain/field at constant stress
  • Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V, strain/field at constant stress
  • Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N, field/stress at constant charge density
  • Piezoelectric Planar Coupling Factor, kp
  • Piezoelectric Mechanical Q, Thin Disk
  • Piezoelectric Shear Coupling Factor, k15
  • Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V, strain/field at constant stress
  • Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N, field/stress at constant charge density
  • Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N, field/stress at constant charge density
  • Piezoelectric Transverse Coupling Factor, k31
  • Thermal Conductivity, Literature value for BaTiO3
  • Melting Point, Literature value for BaTiO3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
formerly ITT exelis formerly edo

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.