MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Omnia Plastica Omniamid PA 6 - Akulon 6 - Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. The use of a high viscosity polymer for the extrusion of Akulon 6 stock shapes results in a product with excellent mechanical properties and a very high standard of quality.

Features:

  • Abrasion resistance: even in dusty and demanding environments, it’s one of the best engineering plastics.
  • Toughness: high tensile stress and compressive strength. The shock resistance is good particularly for annealed material.
  • Fatigue-proof: it maintains its features even under continuous stress.
  • Self-lubricating: the friction coefficient is low and generally for sliding applications it does not require lubricators.
  • Ageing resistance and weatherproof.
  • Natural colour.
Weak Point:

It is hygroscopic; it absorbs moisture which means that in time both its mechanical features and dimensions will change. When dry, it is hard and fragile and when moist it becomes more shock resistant and yielding. Machining is easy but automatic lathes should be avoided as the swarf is extremely elastic.

Application:

  • Mechanical: thanks to its features and its low price it is a popular material for "general purposes". Widely used in the mechanical industry to produce gears, cams, pulleys, anti-wear guides and other mechanical parts. It is used also for guides, bearings and wheels in shipbuilding. For outdoor applications, Akulon GX is preferable due to its higher UV stability.
  • Food contact: generally it is not used in contact with food.
  • Electrical: usage in the electrical field is to be avoided as the electrical features change with the moisture content.
  • Chemical: it is resistant to inorganic compounds and solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors:
Available Properties
  • Density, ISO.1183 DIN.53479
  • Moisture Absorption at Equilibrium, 50% relative humidity
  • Water Absorption at Saturation, 23°C
  • Hardness, Rockwell M, ISO2039.2, dry sample
  • Ball Indentation Hardness, ISO2039.1 DIN.53456
  • Tensile Strength at Break, ISO.527 DIN.53455
  • Elongation at Break, ISO.527 DIN.53455
  • Tensile Modulus, ISO.527 DIN.53455
  • Compressive Strength, ISO.899 DIN.53444, 1% strain over 1000 hours
  • Charpy Impact Unnotched, ISO.R179 DIN.53453, 7.5 J
  • Charpy Impact, Notched, ISO179/3C DIN.53453
  • Coefficient of Friction, Dynamic, on dry ground steel; load =0.05MPa; speed =0.6 m/s
  • Volume Resistivity, ISO.93 DIN.53482
  • Dielectric Constant, ISO.250 DIN.53483
  • Dielectric Strength, ISO.243 DIN.53481
  • Dissipation Factor, ISO.250 DIN.53483
  • CTE, linear
  • Thermal Conductivity, DIN.52612
  • Melting Point
  • Maximum Service Temperature, Air, Continuous; 5000 hours based on a tensile stress of 50% at 23° C.
  • Maximum Service Temperature, Air, short period, no load
  • Deflection Temperature at 1.8 MPa (264 psi), ISO.75 DIN.53461
  • Minimum Service Temperature, Air, impact conditions and heavy loads not considered
  • Flammability, UL94
  • Flammability, UL94
  • Oxygen Index, ISO.4589
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Omnia Plastica s.p.a.

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.