MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Norplex-Micarta NP318 Phenolic Cotton Laminate Sheet, NEMA CF  (discontinued **)
Categories: Polymer; Thermoset; Phenolic

Material Notes: This product has been replaced by Norplex-Micarta NP318U

Post-forming canvas phenolic material. NP318’s mechanical and electrical properties are similar to NP310E. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a thread count of not more than 70 threads per inch in both the warp and filler directions. The binder is a modified phenolic resin system, which permits the material to be heated, formed into a shape and cooled under restraint to hold the newly formed shape.

Information provided by Norplex-Micarta

Key Words: Cotton, Phenolic, Micarta, NEMA CF, Post-forming canvas
Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM D570 Condition A
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, ASTM D638 Condition A, CrossWise
  • Tensile Strength, ASTM D638 Condition A, LengthWise
  • Flexural Strength, ASTM D790 Condition A, CrossWise
  • Flexural Strength, ASTM D790 Condition A, LengthWise
  • Flexural Modulus, ASTM D790 Condition A, CrossWise
  • Flexural Modulus, ASTM D790 Condition A, LengthWise
  • Compressive Strength, ASTM D695 Condition A, Flatwise
  • Shear Strength, ASTM D732 Condition A, perpendicular
  • Izod Impact, Unnotched, ASTM D256 Condition E-48/50, CrossWise
  • Izod Impact, Unnotched, ASTM D256 Condition E-48/50, LengthWise
  • Dielectric Strength, ASTM D149 Condition D-48/50
  • Dielectric Strength, ASTM D149 Condition A
  • Dielectric Breakdown, ASTM D149 Condition D-48/50
  • Dielectric Breakdown, ASTM D149 Condition A
  • Arc Resistance, ASTM D495 Conition A
  • Comparative Tracking Index, ASTM D3638
  • UL RTI, Electrical, UL Bulletin 746b
  • UL RTI, Mechanical with Impact, UL Bulletin 746b
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.