MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman Eastman Advantis™ 515-2 40X adhesion promoter
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Eastman Advantis™ 515-2 40X adhesion promoter (40% in solids in Xylene) is a liquid at room temperature. If the solution gels due to storage at low temperatures, it can be re-liquified by warming to 38°C with agitation. Solutions of Advantis 515-2 40X (as supplied) can easily be reduced with xylene, toluene, selected ketones, and ester solvents. It demonstrates good heat resistance and is compatible with a variety of resins. It combines with the resins to give clear solutions and deposit clear films. Advantis 515-2 40X also has excellent adhesion to polypropylene and good-to-excellent adhesion to many other substrates. Advantis 515-2 40X not only adheres to a variety of substrates, but when added to coatings and inks it improves their adhesion to these substrates.

Applications

  • Auto omen
  • Auto refinish
  • Automotive
  • Automotive parts & accessories
  • General industrial coatings
  • Graphic arts
  • Protective coatings

Information provided by Eastman.

Vendors:
Available Properties
  • Density
  • Density, Solid CPO
  • Flash Point, Tag Closed Cup
  • Ignition Temperature, ASTM D2155, Autoignition
  • Gardner Color Number
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.