MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ATI Allegheny Ludlum Type 332 Stainless Steel, UNS N08800
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Type 332 is a nickel and chromium austenitic stainless steel designed to resist oxidation and carburization at elevated temperatures. The nickel content, 32%, makes the alloy highly resistant both to chloride stress corrosion cracking and to embrittlement from precipitation to sigma phase. The general corrosion resistance is excellent. In the solution annealed condition, Type 332 has superior creep and stress rupture properties. Type 332 has been approved as a material of construction under ASME Boiler and Pressure Vessel Code, Section I - Power Boilers, Section III - Nuclear Vessels, Section VIII - Unfired Pressure Vessels.

Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, Typical; after 1800°F Anneal
  • Tensile Strength, Yield
  • Tensile Strength, Yield, Typical; after 1800°F Anneal
  • Elongation at Break
  • Elongation at Break, Typical; after 1800°F Anneal
  • Reduction of Area, Typical; after 1800°F Anneal
  • Modulus of Elasticity, typical of UNS N08800
  • Poissons Ratio, typical of UNS N08800
  • Shear Modulus, typical of UNS N08800
  • Electrical Resistivity
  • Magnetic Permeability, at 200 Oe
  • Curie Temperature
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe, as balance
  • Manganese, Mn
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ATI Allegheny Ludlum, Allegheny Technologies Incorporated

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.