| Petrothene LT573502 exhibits an enhanced balance of stiffness and environmental stress crack resistance. Typical applications include bottles for motor oil, personal care products, and household chemicals. Availability: North America Application: Bottles For Consumer Goods Market: Rigid Packaging Processing Method: Extrusion Blow Molding Attribute: High Stiffness Information provided by LyondellBasell. |