Coating Description: SHS 7174 TWAS is an iron based steel alloy with a nanoscale microstructure that features good resistance to wear, abrasion, impact, corrosion, high temperature erosion and sulfidation attack.Key Performance Characteristics- Excellent corrosion and wear resistance
- High impact resistance
- Especially resistant to elevated temperature sulfidation attack
- Cost-effective option for elevated temperature erosion/corrosion protection of heat exchange tubes in coal fired boilers
Application Process: Twin Wire Arc Spraying (TWAS) Information Provided by The NanoSteel Company, Inc. |