MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %24 hours at 73°F; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 58.6 MPa
@Thickness 3.17 mm
8500 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 15 %
@Thickness 3.17 mm
15 %
@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 93.1 MPa
@Thickness 3.17 mm
13500 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.48 GPa
@Thickness 3.17 mm
360 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 1.33 J/cm
@Thickness 3.17 mm
2.49 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 0.00 - 60 sec0.00 - 60 secPLC 7
Comparative Tracking Index 175 - 250 V175 - 250 VPLC 3
Hot Wire Ignition, HWI 30 - 60 sec30 - 60 secPLC 2
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsPLC 0
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minPLC 3
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FASTM D648
UL RTI, Electrical 125 °C257 °F
UL RTI, Mechanical with Impact 115 °C239 °F
UL RTI, Mechanical without Impact 125 °C257 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 221 - 249 °C430 - 480 °F
Middle Barrel Temperature 266 - 293 °C510 - 560 °F
Front Barrel Temperature 277 - 299 °C530 - 570 °F
Nozzle Temperature 249 - 288 °C480 - 550 °F
Melt Temperature 271 - 299 °C520 - 570 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 4 hour3 - 4 hour48 hours max.
Back Pressure 0.345 - 1.38 MPa50.0 - 200 psi
 
Descriptive Properties
Injection Speed- Edge GateFast
Injection Speed- Tab GateFast
Injection Speed- Tunnel GateFast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek WCB UNS J13345 Cast Alloy Steel
MetalTek WCC Cast 105-85 Alloy Steel
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
Overview of materials for Polycarbonate, Molded

PZ9PT80 / 21513

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.