MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wellman ThermaClear® Ti818 (0.79 IV) PET  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: ThermaClearTI® Ti818 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. Its titanium catalyst and copolymer formulation provide outstanding clarity and the processing capability needed to achieve high filling temperatures for food packaging. ThermaClearTI® Ti818 may be used in contact with food in full compliance with the Federal Food, Drug, and Cosmetic Act and applicable food additive regulations including 21 CFR Section 177.1630.

Information provided by DAK Americas. Wellman is a subsidiary of DAK Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 56.0 lb/ft³nominal
Viscosity Measurement 0.77 - 0.81BD-61201-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 °CBD-61305
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Chip Size0.24 - 0.44 gm/20 chipsBD-61223
Color-5.0 - -1.0b*, BD-66060
 75.5-79.5L*, BD-66060
Compounds<2 ppmAcetaldehyde, measured on chip, BD-61301

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
DAK Americas Laser+® C91A PET
Celanese Rynite® 408 NC010 PET (Extended Tabular Temperature Data)
Aluminum 6061-O
CENTROPLAST CENTROLYTE FG Polyethylene terephthalate, Food Grade

PDAKA022 / 147997

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.