MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ASI® Pipe Sealer Torque GM 40 Anaerobic Methacrylate Ester Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Torque GM 40 is an anaerobic for sealing of flat mating surfaces and flange joints of pumps, gearboxes, camshafts bocks, motor flanges. To replace pre-formed gaskets, allows greater machining tolerances, assures metal to metal contacting and dismantling with normal tools. Highly resistant to vibrations, heat, water, gases, LPG, oils, hydrocarbons and many chemicals.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
@Temperature 25.0 °C
uncured
Brookfield Viscosity 20000 cP
@Temperature 25.0 °C
Uncured. Spindle 2- 5 rpm
Storage Temperature 8.00 - 28.0 °Cuncured
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 870 - 1160 psiASTM D2095
Shear Strength 725 - 1450 psiASTM D1002
Impact 5.0 - 104-8 Nmm^2
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
Flash Point >= 100 °Cuncured
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 6.00 hourfunctional
 15.0 - 30.0 minhandling.
Shelf Life 12.0 Month
@Temperature 20.0 °C
uncured
 
Descriptive Properties
Chemical ClassMethacrylate Ester
Color / appearanceRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9212 / 233578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.