MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotchcal™ 3690 Graphic Film
Categories: Polymer; Film

Material Notes: This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some low surface energy materials. Designed with a gray-pigmented adhesive for good hiding power, this permanent film provides long term durability in sever weather and handling conditions encountered by commercial and industrial graphics.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milwithout adhesive
 3.00 - 4.00 milwith adhesive
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 17.2 MPa
Peel Strength 3.00 - 6.00 pliAdhesion to Powder coat paint
 5.00 pliAdhesion to ABS
 5.00 pliAdhesion to Acrylic enamel
 5.00 pliAdhesion to Aluminum, etched
 5.00 pliAdhesion to Chrome
 5.00 pliAdhesion to Fiberglass
 6.00 pliAdhesion to Aluminum, anodized
 
Processing PropertiesOriginal ValueComments
Processing Temperature 4.00 - 32.0 °CApplication Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotchcal™ 3690LF Graphic Film
3M ScotchCal™ 3690E Graphic Film Material

PMM34999 / 169746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.