Calcined Bauxite. Hydraulic bond. A low cement, bauxite 1550°C castable with high strengths at all temperatures, low porosity and excellent abrasion, impact and alkali resistance. Silicon Carbide addition increases its resistance to slag and molten metal contact. Applications: Suitable in contact with molten cast iron. Information provided by Morgan Advanced Materials |