MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Gas Compressor Oil ISO Grade 100
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Gas Compressor Oil is a high-quality lubricant developed for the lubrication of oil-flooded rotary compressors in natural gas service and for cylinder lubrication in reciprocating compressors in natural gas service. It is formulated to minimize the effects of gas dilution and oil absorption in this type of service. Gas Compressor Oil is specially formulated to provide excellent service and protection in gas compression service. It has excellent oxidation resistance and thermal stability at high temperatures to help minimize deposit formation and provide long service life. It protects against rust, corrosion and wear, and is resistant to excessive foam buildup that can interfere with proper lubrication.

Applications:

  • Oil-flooded rotary screw, rotary lobe, and rotary vane compressors in natural gas service
  • Industrial reciprocating compressors pumping natural gas
  • Reciprocating compressors commonly found in remote gas gathering stations
Features/Benefits:
  • Excellent oxidation resistance and thermal stability at high temperatures
  • Formulated to minimize the effects of gas dilution and oil absorption
  • Good wear protection
  • Protects against rust and corrosion
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.874 g/cc0.874 g/cc
Density 0.872 g/cc0.0315 lb/in³
Viscosity Measurement 102102Index
Saybolt Viscosity at 100°F 508 SUS508 SUS
Saybolt Viscosity at 210°F 65 SUS65 SUS
Kinematic Viscosity at 40°C (104°F) 97.6 cSt97.6 cSt
Kinematic Viscosity at 100°C (212°F) 11.3 cSt11.3 cSt
ASTM Color 1.51.5ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.140.14[mg KOH/g]; ASTM D974
 
Thermal PropertiesMetricEnglishComments
Pour Point -29.0 °C-20.2 °F
Flash Point 268 °C514 °FCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility5 minutes to pass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5363 / 198616

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.