MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastic Compounds Torlen® PE-2X-901 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: A high-density polyethylene composite material with carbon and stabilizing additives. Designed for extrusion of anti-corrosive surfaces of steel pipes.

Information provided by Polyplastic Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ISO 1183
Environmental Stress Crack Resistance 1000 hour1000 hourISO 16770
Oxidative Induction Time (OIT) 90 min90 minISO 11357-6
Melt Flow 2.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.0 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 24.0 MPa3480 psiISO 527
Tensile Strength, Yield 18.0 MPa2610 psiISO 527-1
Elongation at Break 600 %600 %ISO 527-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FISO 11357
Brittleness Temperature -70.0 °C-94.0 °FISO 11357
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 240 °C428 - 464 °Fat extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPLC152 / 307224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.