MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BYK Fulcat® 220 Clay Catalyst and Adsorbent
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fulcat® 220 is an acid activated Montmorillonite clay catalyst and adsorbent. Acid activation of the natural clay structure develops enhanced Lewis and Brönsted acid sites together with a high surface area that combine to be suitable for a wide range of acid catalyzed reactions. The high surface area of Fulcat® 220 also delivers a product with excellent adsorption properties

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 54.9 lb/ft³
Particle Size >= 5.0 µm10% less than
 40 - 60 µm50% less than
 <= 120 µm90% less than
Specific Surface Area 240 m²/g
 
Chemical PropertiesOriginal ValueComments
Acid Value 28[mg KOH/g}
 
Component Elements PropertiesOriginal ValueComments
Al2O3 15 %
Fe2O3 6.0 %
Free Water 3.0 - 9.0 %
Loss on Ignition(%) 7.5 %
MgO 2.9 %
Na2O 0.30 %
SiO2 64 %
 
Descriptive Properties
Pore volume0.3 cm3/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Cloisite® Ca++ Bentonite
BYK Cloisite® 93A Nanoclay
BYK Cloisite® 93 Salt with bentonite
BYK Cloisite® 5 Salt with bentonite
BYK Cloisite® 30B Nanoclay

PBYK046 / 185043

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.