MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Saint-Gobain Versilon™ C-210-A Precision Polyurethane Tubing Formulation
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Formerly Tygothane® C-210-A. This flexible polyurethane tubing has consistently tight tolerances from lot to lot. Precision tolerances and high elasticity provides an easy, worry-free attachment to fittings. Made of a tough, ester-based polyurethane, Tygothane® Precision Polyurethane Tubing's clarity, high tear strength and excellent abrasion resistance make it ideal for many applications, including fuel and lubricant lines, pneumatic lines, abrasive product transfer and cable jacketing. It also offers exceptional resistance to oils, greases, fuels and many chemicals. Able to withstand rugged daily use, Tygothane® Precision Polyurethane Tubing resists weathering and can be safely used in temperatures ranging from -100°F (-73°C) to 200°F (93°C). It meets FDA criteria for food and beverage use and is also available in ether-based, medical grade and reinforced formulations.

Features/Benefits:
  • Consistently tight dimensional tolerances
  • Excellent abrasion and tear resistance
  • Excellent resistance to oils, greases and fuels
  • High tear resistance
  • Retains flexibility in sub-zero environments
  • Meets FDA criteria
Typical applications include Food and Cosmetic Processing, Abrasive and Viscous Slurry Transfer, Lubrication and Degreaser Dispensing, pellet and Powder Transfer, Pneumatic Sensory Devices, Instrumentation Control Lines, Coolant Recovery Systems
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792-98
Water Absorption 1.12 %24 hours at 23°C; ASTM D570-98
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8215 seconds; ASTM D2240-97
Tensile Strength, Yield 6050 psiASTM D412-98
Elongation at Break 500 %ASTM D412-98
100% Modulus 0.800 ksi
@Strain 100 %
ASTM D412-98
300% Modulus 1.50 ksi
@Strain 300 %
ASTM D412-98
Tear Strength 475 pliInitial Tear Strength; ASTM D1004-94
Compression Set 68 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-98 Method B
Tensile Set 98 %ASTM D412-98
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 330 V/milASTM D149-97
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 175 °F
 200 °FIntermittent
Brittleness Temperature -100 °FASTM D746-98
 
Descriptive Properties
ColorTransparent Natural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® PS 443-201 TPU-Polyester
Syensqo (Solvay Specialty Polymers) Hyflon® MFA® P6310 Perfluoropolymer
Ensinger Tecamid® 6/6 Nylon (PA66)
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A

PSTGQZ204 / 68718

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.