MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC ULTEM™ Resin ATX200 Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D792
Density 1.26 g/cc0.0455 lb/in³ISO 1183
Moisture Absorption 0.500 %0.500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.90 %0.90 %ISO 62-1
Viscosity 16 cP
@Load 5.00 kg,
Temperature 340 °C
16 cP
@Load 11.0 lb,
Temperature 644 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 24 g/10 min
@Load 6.60 kg,
Temperature 337 °C
24 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 125 MPa18100 psiH358/30; ISO 2039-1
Tensile Strength at Break 75.0 MPa10900 psi50 mm/min; ISO 527
 85.0 MPa12300 psi5 mm/min; ASTM D638
Tensile Strength, Yield 95.0 MPa13800 psi50 mm/min; ISO 527
 96.0 MPa13900 psi5 mm/min; ASTM D638
Elongation at Break 20 %20 %50 mm/min; ISO 527
 70 %70 %5 mm/min; ASTM D638
Elongation at Yield 6.5 %6.5 %50 mm/min; ISO 527
 7.0 %7.0 %5 mm/min; ASTM D638
Tensile Modulus 3.00 GPa435 ksi1 mm/min; ISO 527
 3.30 GPa479 ksi5 mm/min; ASTM D638
Flexural Strength 125 MPa18100 psiyield, 2 mm/min; ISO 178
 145 MPa21000 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.10 GPa450 ksi2 mm/min; ISO 178
 3.17 GPa460 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
 55.0 J
@Temperature -30.0 °C
40.6 ft-lb
@Temperature -22.0 °F
ASTM D256
 2136 J
@Thickness 3.20 mm
1575 ft-lb
@Thickness 0.126 in
reverse notched; ASTM D256
Izod Impact, Unnotched 20.82 J/cm39.00 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 J36.9 ft-lbASTM D3763
Taber Abrasion, mg/1000 Cycles 2020CS-17, 1 kg; SABIC method
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 50.0 - 60.0 Hz
2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dissipation Factor  0.0010
@Frequency 50.0 - 60.0 Hz
0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 100 - 175 V100 - 175 VUL 746A
 150 V150 VIEC 60112
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=0.750 mm
>= 120 sec
@Thickness >=0.0295 in
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=0.750 mm
0.00 - 15 arcs
@Thickness >=0.0295 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  50.0 µm/m-°C
@Temperature -40.0 - 150 °C
27.8 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow  50.0 µm/m-°C
@Temperature -40.0 - 150 °C
27.8 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 195 °C383 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 187 °C
@Thickness 3.20 mm
369 °F
@Thickness 0.126 in
unannealed; ASTM D648
 190 °C
@Thickness 6.40 mm
374 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 200 °C392 °FRate B/50; ISO 306
 205 °C401 °FRate B/120; ISO 306
 209 °C408 °FRate B/50; ASTM D1525
 210 °C410 °FRate A/50; ISO 306
UL RTI, Electrical 115 °C239 °FUL 746B
UL RTI, Mechanical with Impact 115 °C239 °FUL 746B
UL RTI, Mechanical without Impact 115 °C239 °FUL 746B
Flammability, UL94  V-2
@Thickness >=0.750 mm
V-2
@Thickness >=0.0295 in
UL 94
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 340 - 360 °C644 - 680 °F
Zone 2 330 - 350 °C626 - 662 °F
Zone 3 340 - 360 °C644 - 680 °F
Melt Temperature 340 - 380 °C644 - 716 °FInjection Molding
Mold Temperature 125 - 140 °C257 - 284 °F
Drying Temperature 130 - 140 °C266 - 284 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
Precipitation Temperature 80.0 - 100 °C176 - 212 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82648 / 290595

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.